宣布日期:2018-06-17 阅读次数:70

厂房普通请求防滑,耐磨,抗压且易清算特色,是以挑选是最适合的。按照厂房空中情况挑选适合的施工工艺。环氧薄涂,环氧沙浆,等。空中情况较差,普通挑选2.0mm环氧沙浆地坪或3.0mm环氧沙浆地坪;挑选环氧自流平也可行,只是造价微高,但做出来的结果雅观,抗压性和耐磨损性是最好的,且操纵年限久长。空中情况较好,新空中,普通较简略的工艺是薄涂地坪和沙浆地坪,因为常常走叉车地牛,倡议在面涂施工后涂刷罩光清漆,如许就能够抗划伤,不易破坏地坪漆。

The epoxy floor of factory building generally requires anti-skid, wear-resistant, compressive and easy cleaning characteristics, so the epoxy floor is the most suitable choice. The suitable construction technology is selected according to the ground condition of the workshop. Epoxy thin coated floor, epoxy mortar floor, epoxy self-leveling floor, etc. Ground condition is poor, generally choose 2.0 mm epoxy mortar floor or 3.0 mm epoxy mortar floor; choose epoxy self-leveling is also feasible, but the cost is slightly high, but the effect is beautiful, compressive and wear resistance is the best, and the service life is long. The ground condition is better, the new ground, generally the simpler process is thin coated floor and mortar floor. Because forklift cattle are often used, it is recommended to apply varnish after surface painting, so as to resist scratches and not easy to damage the floor paint.

涂刷做法:

Brushing method of epoxy floor paint:

①空中打磨清算清洁;

The ground is polished and cleaned.

②涂刷高效环氧底漆一道,涂料要足,完整封底;

(2) Paint a high-efficiency epoxy primer, the paint should be sufficient, completely sealed;

③刮涂无溶剂中涂层沙浆,(这道工序也能够不必,若是操纵会加强地坪的硬度和操纵年限)

(3) Scraping solventless coated mortar, (this process can also not be used, if used will enhance the hardness of the floor and service life)

④刮涂环氧腻子两道;

Fourthly, scrape and coat epoxy putty in two ways.

⑤涂刷两遍环氧面漆。

(5) Brush the epoxy finish twice.

⑥涂刷罩光清漆(这道工序可选)

_Brushing varnish (this process is optional)